Bagasse Ash of Sugar Cane, Hot Mix Asphalt, Latasir BAbstract
From year to year the Portland cement ( PC ) are known to have the price up and down. The Portland cement ( PC ) is used as a filler for asphalt mix is very limited , so it sought an alternative to the use of filler . The existence of abundant ash bagasse in sugar mills Indonesia is still not utilized properly . For now bagasse ash in Indonesian factories only used as fertilizer for sugarcane . This study aims to investigate the performance of hot mix asphalt ( HOT MIX ) LATASIR type - B ( HRSS - B ) with bagasse ash as filler material substitution using a variation of the collision. Specimens are made comprised of three major groups , namely : the test specimen using cement and bitumen of penetration 80/100 ( PC ) , the test object using bagasse ash and bitumen of penetration 80/100 with ( U.S. ) and the test object using the ash residue cane with a variation of the collision and penetration bitumen 80/100 with ( U.S. ) . Total specimen made amounted to 45 , for each type of mixture made 15 test specimens . For ( PC ) Levels of asphalt used is at 6.90% , 7.90% , 8.90 % , 9.90 % , and 10.90 % . Specifications are used to follow the standard Ministry of Settlements and Regional Infrastructure in 2001 using the Marshall method. Filler levels for each of the mixtures was 8.13% and 7.40% OBC generated . For ( AT ) levels fiiler used is 5.00 % , 10.00 % , 15.00 % , 20.00 % , and 25.00 % OBC for each - each mixture was 7.40% and the resulting levels of filler optimum bagasse ash of 7.10 % . Characteristic strength of the mixture based on the value of the stability conditions of the OBC and optimum filler levels . Carrying capacity of filler cement ( PC ) in a mixture of filler OBC 7.40% 8.13% yield and stability of the value of 720 kg , the carrying capacity of bagasse ash ( AT ) in a mixture of 7.40% OBC and filler 7.10% yield stability values 823.35 kg , while carrying a mixed impact on OBC 45 7.40% 7.10 % filler and produce value stability 840.66 kg.
Downloads
Downloads
Published
How to Cite
Issue
Section
License
Copyright (c) 2016 Alik Ansyori Alamsyah, Hari Eko Meiyanto
This work is licensed under a Creative Commons Attribution-ShareAlike 4.0 International License.
Authors who publish with this journal agree to the following terms:
- Authors retain copyright and grant the journal right of first publication with the work simultaneously licensed under a Creative Commons Attribution-ShareAlike 4.0 International License that allows others to share the work with an acknowledgment of the work's authorship and initial publication in this journal.
- Authors are able to enter into separate, additional contractual arrangements for the non-exclusive distribution of the journal's published version of the work (e.g., post it to an institutional repository or publish it in a book), with an acknowledgment of its initial publication in this journal.
- Authors are permitted and encouraged to post their work online (e.g., in institutional repositories or on their website) prior to and during the submission process, as it can lead to productive exchanges, as well as earlier and greater citation of published work (See The Effect of Open Access).
MEDIA TEKNIK SIPIL Journal
This work is licensed under a Creative Commons Attribution-ShareAlike 4.0 International License.